High-collapsibility and recoverable silicon oxide-based ceramic core as well as preparation method and application of high-collapsibility and recoverable silicon oxide-based ceramic core

The invention provides a high-collapsibility and recoverable silicon oxide-based ceramic core as well as a preparation method and application thereof. The high-collapsibility and recoverable silicon oxide-based ceramic core is prepared from the following raw materials: quartz glass basic powder, wat...

Full description

Saved in:
Bibliographic Details
Main Authors QIN YI, ZHAO TING, ZHANG PEI, CHENG YANI, ZHU JIANFENG, FANG YUAN
Format Patent
LanguageChinese
English
Published 01.03.2022
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention provides a high-collapsibility and recoverable silicon oxide-based ceramic core as well as a preparation method and application thereof. The high-collapsibility and recoverable silicon oxide-based ceramic core is prepared from the following raw materials: quartz glass basic powder, water glass, a pore forming agent, an additive and water, the quartz glass base powder is powder obtained by grain composition of nanoscale silicon dioxide and micron-sized silicon dioxide, and the nanoscale silicon dioxide accounts for 10%-75% by mass, and the micron-sized silicon dioxide accounts for 25%-90% by mass; the additive is ceramic powder for inhibiting sintering densification of the quartz glass basic powder; the addition amounts of the water glass, the pore-forming agent, the additive and the water are respectively 1%-8%, 0-15%, 0-40% and 5%-15% of the mass of the quartz glass base powder. The ceramic core is directly preheated and poured without degreasing or dewaxing, is high in collapsibility and can b
Bibliography:Application Number: CN202111426025