Deoxidation slagging material and preparation method thereof

The invention discloses a deoxidation slagging material and a preparation method thereof. The material comprises the following components in percentage by mass: 20-40% of aluminum powder, 20-40% of calcium oxide, 0.1-10% of boron carbide, 0.1-10% of calcium fluoride, 0.1-10% of sodium oxide and the...

Full description

Saved in:
Bibliographic Details
Main Authors GUO YANLONG, TIAN YINLIANG, LIU YUN, DENG JIAXIANG
Format Patent
LanguageChinese
English
Published 30.11.2021
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a deoxidation slagging material and a preparation method thereof. The material comprises the following components in percentage by mass: 20-40% of aluminum powder, 20-40% of calcium oxide, 0.1-10% of boron carbide, 0.1-10% of calcium fluoride, 0.1-10% of sodium oxide and the balance of silicon dioxide. The preparation method of the material comprises the following steps: uniformly mixing and stirring calcium oxide powder and water to prepare calcium oxide slurry; adding the aluminum powder into the calcium oxide slurry, fully mixing and uniformly stirring, cooling, drying and crushing to obtain porous particles; and fully mixing the granular boron carbide, calcium fluoride and silicon dioxide, the porous particles and the sodium oxide to obtain a target product. The deoxidation slagging material is good in deoxidation effect, fast in slagging and easy to clean. 本发明公开了一种脱氧造渣材料及其制备方法,该材料中各成分的质量百分比为:20-40%的铝粉、20-40%的氧化钙、0.1-10%的碳化硼、0.1-10%的氟化钙、0.1-10%的氧化钠,余量为二氧化硅。该材料的制备方法为:将氧化钙粉与水混合搅拌均匀制成
Bibliography:Application Number: CN202111064664