Material for realizing relaxation-normal ferroelectric phase change through doping, and method thereof

The invention discloses a material for realizing relaxation-normal ferroelectric phase change through doping, and a method thereof. The chemical formula of the material is (1-x)SBN-xNN (x = 0-0.8). Na<+> in the material occupies an A-site lattice position which is not occupied by Sr<2+>...

Full description

Saved in:
Bibliographic Details
Main Authors ZHANG SHANTAO, HE XIAOJUAN, GU ZHENGBIN, ZHANG YICHI
Format Patent
LanguageChinese
English
Published 19.11.2021
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a material for realizing relaxation-normal ferroelectric phase change through doping, and a method thereof. The chemical formula of the material is (1-x)SBN-xNN (x = 0-0.8). Na<+> in the material occupies an A-site lattice position which is not occupied by Sr<2+> and Ba<2+> in a tungsten bronze structure, when x is equal to 0, the material is of a non-filled tungsten bronze structure, when x is equal to 0.4, the material is of a filled tungsten bronze structure, and when x is greater than 0.4, the material has a tungsten bronze and perovskite two-phase coexisting composite structure. The method comprises the following steps: synthesizing single-phase SBN powder by adopting a two-step solid-phase reaction method, uniformly mixing the single-phase SBN powder with Na2CO3 and Nb2O5 powder, and sintering at high temperature to obtain the corresponding ceramic material. By doping NN, the SBN crystal structure is converted from a non-full type to a full type, relaxation-normal ferroelectric p
Bibliography:Application Number: CN202111002354