The invention discloses a production method for improving wear resistance of a heat-treated steel rail. The production method comprises the step of carrying out dynamic accelerated cooling heat treatment on a hot-rolled steel rail head, wherein the initial cooling temperature is controlled to be 720...

Full description

Saved in:
Bibliographic Details
Main Authors ZHENG JIANGUO, WANG JUN, OUYANG MINLU, FEI JUNJIE, DONG MAOSONG, ZHOU JIANHUA, ZHU MIN
Format Patent
LanguageChinese
English
Published 17.09.2021
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a production method for improving wear resistance of a heat-treated steel rail. The production method comprises the step of carrying out dynamic accelerated cooling heat treatment on a hot-rolled steel rail head, wherein the initial cooling temperature is controlled to be 720-800 DEG C, a dynamic stage cooling process is adopted, namely the whole rail head cooling process is divided into seven stages, the cooling speed of the first stage is 5-7 DEG C/s, the cooling speed of the second stage is 7-8 DEG C/s, the cooling speed of the third stage is 8-10 DEG C/s, the cooling speed of the fourth stage is 1-2 DEG C/s, the cooling speed of the fifth stage is 4-6 DEG C/s, the cooling speed of the sixth stage is 3-4 DEG C/s, the cooling speed of the seventh stage is 2-3 DEG C/s, when the temperature of the rail head is reduced to 300 DEG C or below, accelerated cooling is stopped, and finally natural cooling is conducted to the room temperature. According to the production method, by reasonably
Bibliography:Application Number: CN202110576248