Method for preventing perforated adhesive film from deforming after cutting

The invention discloses a method for preventing a perforated adhesive film from deforming after cutting. The method comprises the following steps that S1, cutter machining is performed, specifically, the width of a central hole (2) in an adhesive film blank (5) is measured, an arc-shaped groove (8)...

Full description

Saved in:
Bibliographic Details
Main Authors FANG HUA, BAI YUANSHENG, YANG CHENG, SHI AN, CHEN SHIBIN, LI YUNSHI
Format Patent
LanguageChinese
English
Published 28.05.2021
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a method for preventing a perforated adhesive film from deforming after cutting. The method comprises the following steps that S1, cutter machining is performed, specifically, the width of a central hole (2) in an adhesive film blank (5) is measured, an arc-shaped groove (8) is milled in the right end surface of a straight cutter, the width of the arc-shaped groove (8) is guaranteed to be larger than that of the central hole (2), and meanwhile, the lower edge of the arc-shaped groove (8) is guaranteed to penetrate through a cutting edge (9) of the straight cutter, so that the cutter (10) is machined; and S3, the cutter (10) is adopted to downwards cut the left end portion of the adhesive film blank (5), the cutting edge (9) of the cutter (10) is cut into the adhesive film blank (5), part of a material of the left end portion of the adhesive film blank (5) is contained in the arc-shaped groove (8), and an arc-shaped protrusion (13) matched with the arc-shaped groove (8) is formed on the
Bibliography:Application Number: CN202011490188