Light heat insulation ceramic tile and preparation method thereof

The invention discloses a light heat insulation ceramic tile and a preparation method thereof. The light heat insulation ceramic tile is prepared from, by weight, 30-50 parts of red mud, 5-20 parts ofyellow mud, 20-40 parts of sand, 10-20 parts of weathered mud cake, 10-25 parts of fine mud cake and...

Full description

Saved in:
Bibliographic Details
Main Authors JIAN WEICHUANG, HUANG JINMING, HUANG TINGTING
Format Patent
LanguageChinese
English
Published 05.03.2021
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a light heat insulation ceramic tile and a preparation method thereof. The light heat insulation ceramic tile is prepared from, by weight, 30-50 parts of red mud, 5-20 parts ofyellow mud, 20-40 parts of sand, 10-20 parts of weathered mud cake, 10-25 parts of fine mud cake and 0-10 parts of sawdust powder. The fine mud cake comprises powder waste residues of granite and powder waste residues of quartzite. The preparation method of the light heat insulation ceramic tile comprises the following steps: (1) adding water into the raw materials according to the formula, and conducting uniform mixing to obtain a blank with the water content of 18-20% according to the weight ratio; (2) extruding and stamping the blank into a blank body by a vacuum pugging wet method; and (3) conducting firing, wherein the temperature curve of high-temperature firing comprises that the temperature is increased from 260 DEG C to 400 DEG C, and the time is consumed for 2.5-3.5 hours; the temperature is increased f
Bibliography:Application Number: CN202011357851