Wear-resistant chlorosulfonated polyethylene rubber and preparation method thereof

The invention discloses wear-resistant chlorosulfonated polyethylene rubber and a preparation method thereof. The wear-resistant chlorosulfonated polyethylene rubber comprises chlorosulfonated polyethylene rubber, S40V chloroprene rubber, phenolic resin, polymethyltriethoxysilane, N-butyl methacryla...

Full description

Saved in:
Bibliographic Details
Main Authors ZHANG PENG, SUN GUIYUAN, CHEN QIAONA
Format Patent
LanguageChinese
English
Published 23.10.2020
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses wear-resistant chlorosulfonated polyethylene rubber and a preparation method thereof. The wear-resistant chlorosulfonated polyethylene rubber comprises chlorosulfonated polyethylene rubber, S40V chloroprene rubber, phenolic resin, polymethyltriethoxysilane, N-butyl methacrylate, zinc oxide, carbon black, a softener, sulfur, polyphenylene sulfide, distilled water, calcium stearate, carboxylic butadiene-acrylonitrile latex, nanometer calcium carbonate, nanometer silicon dioxide, stearic acid, an antioxidant1035, 3-aminopropyltrimethoxysilane, a silane coupling agent KH-550, calcined kaolin, an accelerant CZ, an accelerant CBS, an accelerant Na-22, an anti-aging agent ODA, an anti-aging agent RD, glass fibers and sodium hexametaphosphate. Due to large surface hardness,the wear-resistant chlorosulfonated polyethylene rubber has excellent wear resistance, the compatibility of the wear-resistant chlorosulfonated polyethylene rubber with a rubber matrix is improved toa great extent, a more un
Bibliography:Application Number: CN201910286721