Foamed ceramic prepared from steel slag and preparation method thereof

The invention discloses a foamed ceramic prepared from steel slag and a preparation method thereof, and belongs to the technical field of building materials. The foamed ceramic comprises the followingraw materials in parts by weight: 100-150 parts of steel slag, 25-30 parts of mullite, 30-40 parts o...

Full description

Saved in:
Bibliographic Details
Main Authors CHEN PING, SONG JIEGUANG, LI LIANGSONG, PANG CAILIANG, ZENG QING, XU HAO, LIU RONGJIN, LUO DEPING, YANG XUEQING
Format Patent
LanguageChinese
English
Published 05.06.2020
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a foamed ceramic prepared from steel slag and a preparation method thereof, and belongs to the technical field of building materials. The foamed ceramic comprises the followingraw materials in parts by weight: 100-150 parts of steel slag, 25-30 parts of mullite, 30-40 parts of silicon dioxide, 20-30 parts of ferric oxide, 15-20 parts of graphite, 5-15 parts of river sand,25-55 parts of purified water, 5-15 parts of sludge and 5-10 parts of polyacrylamide. The invention further provides a preparation method of the foamed ceramic. The prepared foamed ceramic has good compressive strength, heat conductivity coefficient and closed-pore rate. 本发明公开了一种利用钢渣制备的泡沫陶瓷及其制备方法。属于建筑材料技术领域。包括以下重量份的原料:钢渣100-150份、莫来石25-30份、二氧化硅30-40份、三氧化二铁20-30份、石墨15-20份、河沙5-15份、纯净水25-55份、污泥5-15份和聚丙烯酰胺5-10份,并提供了其制备方法。本发明制备的泡沫陶瓷具有良好的抗压强度、导热系数和闭孔率。