Method for preparing orpiment crystals by hydrothermal method
The invention discloses a method for preparing orpiment crystal by a hydrothermal method, which comprises the following steps: by using amorphous As2S3 as a raw material, carrying out hydrothermal treatment at 180-270 DEG C for 6-48 hours to obtain the orpiment crystal. According to the invention, a...
Saved in:
Main Authors | , , , , , , , , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
05.06.2020
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention discloses a method for preparing orpiment crystal by a hydrothermal method, which comprises the following steps: by using amorphous As2S3 as a raw material, carrying out hydrothermal treatment at 180-270 DEG C for 6-48 hours to obtain the orpiment crystal. According to the invention, amorphous As2S3 is used as a raw material; by strictly controlling the temperature and time of hydro-thermal treatment, amorphous arsenic trisulfide is converted into stable orpiment crystals; by further optimizing the pH, solid-liquid ratio, temperature and time of hydro-thermal treatment, the orpiment crystals are good in crystal form, high in conversion rate and free of other impurities, and controllable synthesis of the orpiment crystals is achieved.
本发明公开了一种水热法制备雌黄晶体的方法,以非晶态三硫化二砷为原料,在温度为180℃~270℃的条件下,水热处理6h~48h得到雌黄晶体。本发明以非晶态三硫化二砷为原料,通过严格控制水热处理的温度和时间,将非晶态三硫化二砷转变为稳定的雌黄晶体,并通过进一步的优化水热处理的pH、固液比、温度和时间,能使得雌黄晶体晶型良好、转化率高、无其他杂质存在,实现了雌黄晶体的可控合成。 |
---|---|