125 DEG C irradiation crosslinked low-smoke halogen-free flame-retardant polyolefin cable material for new energy vehicle
The invention discloses a 125 DEG C irradiation crosslinked low-smoke halogen-free flame-retardant polyolefin cable material for a new energy vehicle. The material is composed of the following components in parts by weight: 100 parts of polyolefin elastomer, 10-18 parts of ethylene-vinyl acetate cop...
Saved in:
Main Authors | , , , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
29.05.2020
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention discloses a 125 DEG C irradiation crosslinked low-smoke halogen-free flame-retardant polyolefin cable material for a new energy vehicle. The material is composed of the following components in parts by weight: 100 parts of polyolefin elastomer, 10-18 parts of ethylene-vinyl acetate copolymer, 30-50 parts of silane modified aluminum hydroxide, 0.5-2 parts of silicone resin, 12-18 parts of silane modified magnesium hydroxide, 3-8 parts of polyethylene wax, 2-4 parts of an antioxidant, 0.5-1.5 parts of a crosslinking agent, 3-5 parts of a styrene-butadiene copolymer, 4-8 parts of polyethylene glycol distearate and 1-3 parts of N-amino phthalimide, wherein the polyolefin elastomer is prepared from 60 to 100 parts by weight of ethylene-octene copolymer, 20 to 50 parts by weight oflinear low-density polyethylene and 10 to 20 parts by weight of ethylene-propylene binary copolymer. Under the thermal aging conditions: IRM902 test oil 168h/100 +/-2 DEG C and 150 DEG C*240h, the retention rate of the tensi |
---|---|
Bibliography: | Application Number: CN202010200284 |