The invention discloses a reducing agent of a propellant. The reducing agent comprises the following ingredients in parts by weight: 8-12 parts of an adhesive, 9.6-14.4 parts of a reducing agent, 6.4-9.6 parts of a conductive reducing agent, 2.4-3.6 parts of an adhesive reducing agent, 2.4-3.6 parts...

Full description

Saved in:
Bibliographic Details
Main Authors GUO HUI, ZHONG CHUNWEN, SONG NIU, YAN HONGLIANG
Format Patent
LanguageChinese
English
Published 15.10.2019
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a reducing agent of a propellant. The reducing agent comprises the following ingredients in parts by weight: 8-12 parts of an adhesive, 9.6-14.4 parts of a reducing agent, 6.4-9.6 parts of a conductive reducing agent, 2.4-3.6 parts of an adhesive reducing agent, 2.4-3.6 parts of a catalyst and 0.4-0.6 parts of a stabilizing agent. In the mixture of the reducing agent, sulfur or sulfides does/do not exist, meanwhile, nitrocotton is not used, therefore, pollution to air is greatly reduced, and the cost is greatly lowered. 本发明公开了一种发射药的还原剂,包括粘合剂8-12重量份;还原剂9.6-14.4重量份;导电还原剂6.4-9.6重量份;粘合还原剂2.4-3.6重量份;催化剂2.4-3.6重量份;稳定剂0.4-0.6重量份。本发明的混合物中不存在硫或硫化物,同时不使用硝化棉,从而在大大降低对空气污染的同时,大大降低了成本。
Bibliography:Application Number: CN201910633331