Highly wear-resistant alloy bar and production technology thereof

The invention relates to a highly wear-resistant alloy bar. The highly wear-resistant alloy bar consists of the following substances in percentage by mass: 0.3-1.8% of C, 1.8-3.5% of Si, 0.8-2.5% of Ti, 1.3-1.5% of Bi, 0.5-1.5% of Mn, 1.1-1.3% of Cr, 0.1-0.5% of Al, 0.1-0.8% of Cu, 0.5-1.5% of Mg, 0...

Full description

Saved in:
Bibliographic Details
Main Authors SONG WENTAO, LU KEYIN, YANG YONGCHUAN, SONG HENGBIN
Format Patent
LanguageChinese
English
Published 12.07.2019
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention relates to a highly wear-resistant alloy bar. The highly wear-resistant alloy bar consists of the following substances in percentage by mass: 0.3-1.8% of C, 1.8-3.5% of Si, 0.8-2.5% of Ti, 1.3-1.5% of Bi, 0.5-1.5% of Mn, 1.1-1.3% of Cr, 0.1-0.5% of Al, 0.1-0.8% of Cu, 0.5-1.5% of Mg, 0.1-1.1% of Ni, 0.05-0.3% of V, 0.01-1.1% of La, 0.01-1.1% of Re, 0.1-3.5% of Mo, 1.2-3.1% of W, andthe balance Fe containing inevitable impurities. A production technology of the highly wear-resistant alloy bar comprises the steps of smelting, casting moulding, surface carburizing and high frequency quenching. On one hand, the highly wear-resistant alloy bar can be effectively produced, the production and preparation technology is simple, raw materials are convenient to obtain and the cost is relatively low. On the other hand, the structural strength, toughness and wear resistance of the bar can be effectively improved, so that the operation and use performance of the bar are greatly improved, the friction loss dur
Bibliography:Application Number: CN201910333650