Continuous reaction method for synthesizing large-particle-size cobalt carbonate

The invention discloses a continuous reaction method for synthesizing large-particle-size cobalt carbonate, which specifically comprises the following steps: respectively preparing a cobalt chloride solution with a concentration of 10-120 g/L and a sodium bicarbonate solution with a concentration of...

Full description

Saved in:
Bibliographic Details
Main Authors XU DONGWEI, SHI QIYONG, XU KAIHUA, FAN YEYE, ZHANG AIQING, LI BINGZHONG, WU YIGEN
Format Patent
LanguageChinese
English
Published 09.07.2019
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a continuous reaction method for synthesizing large-particle-size cobalt carbonate, which specifically comprises the following steps: respectively preparing a cobalt chloride solution with a concentration of 10-120 g/L and a sodium bicarbonate solution with a concentration of 50-130 g/L, and pumping the prepared cobalt chloride solution into a reaction kettle to serve as abase solution; continuously pumping the cobalt chloride solution into the reaction kettle, heating the solution in the reaction kettle to 50-70 DEG C, pumping the sodium bicarbonate solution into thereaction kettle to adjust the pH value to 5.0-8.5, and stirring the solution in the reaction kettle for reaction; and when the solid content in the solution in the reaction kettle reaches 150-300 g/L,stopping pumping the cobalt chloride solution and the sodium bicarbonate solution, standing and aging the obtained turbid liquid, and conducting filtering, washing and drying to obtain a finished product. According to the proc