Modified perlite gunning repairing material and preparation method thereof

The invention discloses a modified perlite gunning repairing material and a preparation method thereof. The preparation method comprises the following steps: firstly, mixing waste brick granules, lignocelluloses and perlite, then sequentially adding hexamethylenetetramine, magnesium oxide and sodium...

Full description

Saved in:
Bibliographic Details
Main Authors LU JUN, CAI ZHONGDONG, CHEN JIE, WANG JING, YU GENXIN, LU MINGGEN
Format Patent
LanguageChinese
English
Published 26.04.2019
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a modified perlite gunning repairing material and a preparation method thereof. The preparation method comprises the following steps: firstly, mixing waste brick granules, lignocelluloses and perlite, then sequentially adding hexamethylenetetramine, magnesium oxide and sodium tripolyphosphate, stirring uniformly, heating to 40-45 DEG C, and reacting for 20-40 minutes; adding sodium silicate and water, uniformly stirring to obtain the modified perlite gunning repairing material. Due to adoption of modified perlite, the pressure resistance and the fracture resistance canbe remarkably improved, and the pressure resistance under a high temperature condition is not greatly degraded. The particle size of the waste brick granules is controlled within 0.3-1mm, so that thepressure resistance of the material is slightly degraded, and the pressure resistance is not greatly degraded even under the high temperature condition. 本发明公开了一种改性珍珠岩喷补料及其制备方法,该方法包括以下步骤:先将废砖颗粒、木质纤维素和珍珠岩混合,再依次加入六亚甲基四胺、氧化镁和三聚磷酸钠
Bibliography:Application Number: CN201910069124