Enhancement modified building plaster
The invention relates to enhancement modified building plaster which is prepared from the following raw materials in percentage by weight through uniform mixing and dry mixing: 65-80% of building plaster, 15-30% of anhydrite and 3-5% of an enhancement modifier. By adopting the building plaster, the...
Saved in:
Main Authors | , , , , , , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
26.02.2019
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention relates to enhancement modified building plaster which is prepared from the following raw materials in percentage by weight through uniform mixing and dry mixing: 65-80% of building plaster, 15-30% of anhydrite and 3-5% of an enhancement modifier. By adopting the building plaster, the strength of a plaster hydration hardening body is greatly improved, the plaster has good mechanicalproperties, and the problem that building plaster self is low in strength can be effectively solved.
本发明涉及种增强改性的建筑石膏,按重量百分比计,由下述原料混合干拌均匀制得:65%~80%建筑石膏,15%~30%无水石膏,3~5%增强改性剂。本发明大幅提高了石膏水化硬化体的强度,使其具有较好的力学性能,有效解决了建筑石膏自身强度低的问题。 |
---|---|
Bibliography: | Application Number: CN201811475684 |