Fireproof coating for cables and preparation method thereof
The invention discloses fireproof coating for cables and a preparation method thereof. The fireproof coating is prepared by mixing the following raw materials in parts by weight: 100 to 120 parts of acoating matrix, 30 to 40 parts of composite filling, 20 to 30 parts of a flame retardant, 20 to 30 p...
Saved in:
Main Author | |
---|---|
Format | Patent |
Language | Chinese English |
Published |
25.01.2019
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention discloses fireproof coating for cables and a preparation method thereof. The fireproof coating is prepared by mixing the following raw materials in parts by weight: 100 to 120 parts of acoating matrix, 30 to 40 parts of composite filling, 20 to 30 parts of a flame retardant, 20 to 30 parts of emulsified silicone oil, 4 to 8 parts of antimony trioxide, 8 to 12 parts of nano titaniumdioxide, 6 to 10 parts of graphite powder, 3 to 6 parts of zinc borate, 2 to 5 parts of organic bentonite, 5 to 8 parts of titanium dioxide, 5 to 10 parts of dimethicone, 15 to 20 parts of an auxiliary agent and 50 to 80 parts of de-ionized water. The fireproof coating prepared by the method has high toughness, good bending resistance and alkali resistance, strong adhesive force and good flame-retarding and insulation performance, and has a very good protection effect on the cables; the service life of the cables can be effectively prolonged and the safety is improved.
本发明公开了种用于电缆的防火涂料及其制备方法,所述防火涂料包括以下按重量份配比的原料混合组成:涂料基 |
---|---|
Bibliography: | Application Number: CN201811093768 |