Bark glaze and preparation method
The invention discloses a bark glaze and a preparation method. A glaze material of the bark glaze comprises the following components of 15-20 parts of feldspar powder, 20-25 parts of barium carbonate,20-25 parts of calcite, 5-10 parts of magnesium carbonate, 2-5 parts of calcined talcum, 15-20 parts...
Saved in:
Main Author | |
---|---|
Format | Patent |
Language | Chinese English |
Published |
08.01.2019
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention discloses a bark glaze and a preparation method. A glaze material of the bark glaze comprises the following components of 15-20 parts of feldspar powder, 20-25 parts of barium carbonate,20-25 parts of calcite, 5-10 parts of magnesium carbonate, 2-5 parts of calcined talcum, 15-20 parts of zinc oxide and 6-12 parts of titanium oxide in parts by mass. 0.05% of carboxymethylcellulose is added to the glaze material according to mass percentage. The glazed surface of the bark glaze can represent a bark-like response effect, gives people an artistic conception of following the pure nature, makes people temporarily forget the noise of the city to return to the peace of nature and brings consumers a relaxed and happy feeling.
本发明公开了种树皮釉及其制备方法,树皮釉的釉料中含有的组分及各组分的质量份如下:长石粉15-20份,碳酸钡20-25份,方解石20-25份,碳酸镁5-10份,煅烧滑石2-5份,氧化锌15-20份,氧化钛6-12份;在所述釉料中添加质量百分比为千分之五的羧甲基纤维素。树皮釉的釉面能够呈现树皮状反应效果,给人种追求自然返朴归真的意境,它让人暂时忘却城市的喧哗,回归到大自然本来的宁静,带给消费者心旷神怡的感觉。 |
---|---|
Bibliography: | Application Number: CN201811143864 |