Preparing method of negative low aging rate negative temperature coefficient thermistor ceramic material

The invention discloses a preparing method of a negative low aging rate negative temperature coefficient thermistor ceramic material. The nominal chemical composition of the thermistor ceramic material is Mn3-x-y-zNixFeyMzO4, wherein M represents Cu, Ti, Sn, and Al, an oxide for constituting anions...

Full description

Saved in:
Bibliographic Details
Main Authors ZHU SHAOFENG, LI DONGCAI, QIAN NIYAN, LIU BINGCHEN, SHI QING
Format Patent
LanguageChinese
English
Published 17.07.2018
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a preparing method of a negative low aging rate negative temperature coefficient thermistor ceramic material. The nominal chemical composition of the thermistor ceramic material is Mn3-x-y-zNixFeyMzO4, wherein M represents Cu, Ti, Sn, and Al, an oxide for constituting anions serves a starting raw material, ball milling is conducted, after multiple times of roasting, organicbinding agent is added for pelleting molding, sintering is conducted, after sheet-like samples are sintered, silver electrodes are arranged on the two end faces, and after the electrodes are burned and permeate, under an oxygen-enriched environment, the portion, free of electrodes and covered with cylinders, of samples is sealed through middle-temperature vitereous glaze. The thermistor ceramic material prepared through the preparing technology has an electrical resistivity of 3-1,000 ohm.m at the temperature of 25 DEG C, has a B value of 3,000-4,000 K at the temperature of 25-85 DEG C, and has a weekly aging rate of