Highly pure birnessite and method for the production thereof

A method of producing an oxide of manganese including reacting, in a first aqueous solution, a manganese salt and an alkali agent to form manganese hydroxide; separating the manganese hydroxide from the first solution; mixing the manganese hydroxide into an aqueous medium to form a manganese hydroxi...

Full description

Saved in:
Bibliographic Details
Main Authors SCHILLING OLIVER, SOUPART JEAN-BRUNO R. B, REBMANN GUILLAUME B
Format Patent
LanguageChinese
English
Published 16.02.2018
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A method of producing an oxide of manganese including reacting, in a first aqueous solution, a manganese salt and an alkali agent to form manganese hydroxide; separating the manganese hydroxide from the first solution; mixing the manganese hydroxide into an aqueous medium to form a manganese hydroxide suspension; mixing the manganese hydroxide suspension with alkali metal hydroxide to form a second aqueous solution; and oxidizing the manganese hydroxide in the second aqueous solution to form an oxide of manganese. The dried oxide of manganese includes birnessite, a maximum of 20% hausmannite,and a maximum of 10% feitknechtite, may further include a maximum of 400 ppm of anions, may have a specific surface area of at least 25 m /g, and may have an average oxidation state of greater than3.5. 种制造锰的氧化物的方法,包括:在第水溶液中使锰盐和碱性试剂反应以形成氢氧化锰;从所述第水溶液中分离出所述氢氧化锰;将所述氢氧化锰混入水性介质中以形成氢氧化锰悬浮液;将所述氢氧化锰悬浮液与碱金属氢氧化物混合以形成第二水溶液;和氧化所述第二水溶液中的所述氢氧化锰以形成锰的氧化物。该干燥的锰的氧化物包含水钠锰矿、至多20%的黑锰矿和至多10%的六方水锰矿,可以还包含至多400ppm的阴离子,可以具有至少25m/g的比表面积,并且可以具有大于3.5的
Bibliography:Application Number: CN201680036381