Preparation method of silver-tin oxide-wolfram carbide composite electric contact material and product thereof

The invention discloses a preparation method of silver-tin oxide-wolfram carbide composite electric contact material and a product thereof. The technical scheme is characterized in that a basis material of a contact comprises, by weight, 1-20% of tin oxide, 0.01-10% of wolfram carbide, less than 5%...

Full description

Saved in:
Bibliographic Details
Main Authors MIAO RENLIANG, BAI XIAOPING, WAN DAI, LIN WANHUAN, ZHOU KEWU, YAO PEIJIAN
Format Patent
LanguageChinese
English
Published 22.12.2017
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a preparation method of silver-tin oxide-wolfram carbide composite electric contact material and a product thereof. The technical scheme is characterized in that a basis material of a contact comprises, by weight, 1-20% of tin oxide, 0.01-10% of wolfram carbide, less than 5% of additives and the balance silver. The preparation method of the silver-tin oxide-wolfram carbide composite electric contact material and the product thereof has the advantages and the positive effects as follows: 1, a chemical reduction coating method is adopted, so that the uniformity of mixed powder is better and the sintering strength is higher; 2, the surfaces of the WC powder body and the SnO2 powder body are uniformly coated with a silver layer, so that the electric arc erosion resistance and the melt welding resistance of the electric contact material are improved, and the reliability of a contactor is improved; and 3, the Ag-SnO2-WC contact material with appropriate components is selected, so that the ar
Bibliography:Application Number: CN20171630156