Preparation method of sealant 180-degree peel strength sample

The invention relates to a simple method for preparation of a 180-degree peel strength sample during sealant 180-degree peel strength testing after air aging. By using a diluted sealant as a protective coating, the sealant 180-degree peel strength sample prepared according to HB5249-1993 'Room...

Full description

Saved in:
Bibliographic Details
Main Authors ZHANG JINGTONG, LI HUI, WANG YUKUI, ZHANG HAIQING, XU HUIJING, ZHANG HUI, CHEN JUNWEN, WU JUNJUN, XING JIANWEI, XUAN XIAONAN, YANG GENJUN
Format Patent
LanguageChinese
English
Published 01.09.2017
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention relates to a simple method for preparation of a 180-degree peel strength sample during sealant 180-degree peel strength testing after air aging. By using a diluted sealant as a protective coating, the sealant 180-degree peel strength sample prepared according to HB5249-1993 'Room temperature vulcanization sealant 180-degree peel strength test method' will not be aged or brittle after air aging, and the rate of waste samples is reduced. 本发明说明了种热空气老化后测定密封剂180°剥离强度试验时,180°剥离强度试样制备的种简易方法。通过采用稀释的密封剂做为保护涂料,使得按照HB5249-1993《室温硫化密封剂180°剥离强度试验方法》制备的密封剂180°剥离强度试样在经热空气老化后不会老化发脆,使得废样比率降低。
Bibliography:Application Number: CN20161104249