Method for producing malleable iron pipe by using reclaiming waste

The invention relates to a method for producing a malleable iron pipe by using reclaiming waste. The method is characterized in that a medium frequency furnace smelting process is adopted, foundry pig iron with waste machine iron, and raw materials include, by weight, 45-55 parts of foundry returns,...

Full description

Saved in:
Bibliographic Details
Main Authors CHEN XIUJUN, LIU TANG, LIU JINSHENG, AI CHENGUANG, REN FUYAN, CHEN FENGYU
Format Patent
LanguageChinese
English
Published 31.05.2017
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention relates to a method for producing a malleable iron pipe by using reclaiming waste. The method is characterized in that a medium frequency furnace smelting process is adopted, foundry pig iron with waste machine iron, and raw materials include, by weight, 45-55 parts of foundry returns, 10-30 parts of waste rolled steel, 20-35 parts of the machine iron, 0.6-1 part of a carburetant, 0.25-0.5 part of ferrosilicon and 0-10 parts of malleable cast iron chippings. According to the method, the raw material structure and the matching process are optimized, the matrix structure of a cast workblank piece is improved, the product performance is stabilized, the phenomenon of casting grey pieces is reduced, and the rejection rate of cast products is reduced. 种使用回收废料生产可锻铸铁管件的方法,所述方法采用中频电炉熔炼工艺,以废机铁替代铸造生铁,其原料的重量份配比为:回炉料,45~55份;废钢材,10~30份;机铁,20~35份;增碳剂,0.6~1份;硅铁,0.25~0.5份;玛钢屑,0~10份。本发明通过优化原料结构和配比工艺,改善了铸造毛坯件的基体组织,稳定了产品的性能,减少了铸造灰件现象,降低了铸造产品的废品率。
Bibliography:Application Number: CN201611123934