Anti-aging cracking thermal insulation mortar and preparation method thereof
The invention discloses an anti-aging cracking thermal insulation mortar and a preparation method thereof. The mortar is prepared from the following raw materials by weight: 11-19 parts of high titanium slag, 7-14 parts of nano zirconium boride fiber, 14-23 parts of crushed gravel, 5-10 parts of hem...
Saved in:
Main Author | |
---|---|
Format | Patent |
Language | Chinese English |
Published |
09.11.2016
|
Subjects | |
Online Access | Get full text |
Cover
Summary: | The invention discloses an anti-aging cracking thermal insulation mortar and a preparation method thereof. The mortar is prepared from the following raw materials by weight: 11-19 parts of high titanium slag, 7-14 parts of nano zirconium boride fiber, 14-23 parts of crushed gravel, 5-10 parts of hemp cut lime mortar, 4-9 parts of aramid pulp, 8-14 parts of asbestos powder, 10-15 parts of kiln slag, 6-9 parts of hydroxyethylmethylcellulose, 4-7 parts of glucomannan, 41-53 parts of magnesium oxychloride cement, 14-20 parts of tephra, 5-8 parts of triethanolamine alginate, 12-18 parts of waste foam concrete, 16-24 parts of sillimanite, 13-21 parts of pumice, and 4-8 parts of calcium propionate. The prepared thermal insulation mortar has the advantages of excellent anti-aging cracking performance, strong bonding strength, high strength, strong anti-seepage capacity and wide application.
本发明公开了种抗老化开裂保温砂浆及其制备方法,其由以下重量份的原料制成:高钛渣11-19、纳米硼化锆纤维7-14、碎砾石14-23、麻刀灰5-10、芳纶浆粕4-9、石棉粉8-14、炉窑渣10-15、羟乙基甲基纤维素6-9、葡甘露聚糖4-7、氯氧镁水泥41- |
---|---|
Bibliography: | Application Number: CN20161418470 |