Rustproof automobile finish preparation method

The invention discloses a rustproof automobile finish preparation method, and belongs to the technical field of paint manufacturing. The preparation method comprises the steps that on the ultrasonic conditions that the ultrasonic power is 80 W, and the ultrasonic frequency is 45 KHz, epoxy resin, ac...

Full description

Saved in:
Bibliographic Details
Main Authors DONG CHUNXIA, WEI GUANGNAN, LIU ZHANGUANG
Format Patent
LanguageChinese
English
Published 28.09.2016
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a rustproof automobile finish preparation method, and belongs to the technical field of paint manufacturing. The preparation method comprises the steps that on the ultrasonic conditions that the ultrasonic power is 80 W, and the ultrasonic frequency is 45 KHz, epoxy resin, acrylate resin, polyethylene glycol, polyethylether modified trisiloxane and pigment are mixed and subjected to ultrasonic treatment for 15 min to 30 min at 50 DEG C to 60 DEG C; white carbon black, sodium metal, sulfur and cardanol are added, and stirring is conducted for 10 min to 15 min under the ultraviolet light condition. According to the rustproof automobile finish preparation method, under the specific ultrasonic condition at present, epoxy resin, acrylate resin, polyethylene glycol, polyethylether modified trisiloxane and pigment are added for heating and ultrasonic treatment, white carbon black, sodium metal, sulfur and cardanol are added, stirring is conducted under the ultraviolet light condition, and the
Bibliography:Application Number: CN20161359507