More Information
Summary:The invention discloses a centrifugal casting furnace tube and a preparation technology thereof. The preparation technology comprises the following steps: taking steel scrap, ferromanganese and ferrosilicon, ferrochromium, pure nickel, ferromolybdenum and rare earth nickel gadolinium, and nickel cerium intermediate alloy as the raw materials, adopting an aluminium wire for deoxygenation, and deslagging on the liquid level of molten steel to obtain molten-state molten steel; according to the formula N=20*(G/r)<1/2>, calculating the centrifugal rotational speed of a steel tube cavity manufactured through centrifugal casting; when the rotating speed of the steel tube cavity reaches the calculated centrifugal rotational speed, pouring molten steel to the cavity from a steel ladle, and adopting argon during the pouring process to ensure that molten steel is not oxidized, wherein the pouring temperature is 1523-1573 DEG C and the pouring time is about 5-10 minutes; demoulding, cooling a centrifugal steel tube to th
Bibliography:Application Number: CN20161335401