More Information
Summary:A method of sequestering carbon dioxide comprises reacting the carbon dioxide with aqueous magnesium ions at elevated pH to form magnesium carbonate-containing salts. The carbon dioxide is preferably reacted with alkali to form carbonate and/or bicarbonate anions at elevated pH, and the carbonate and/or bicarbonate anions are subsequently reacted with aqueous magnesium cations to form the magnesium carbonate- containing salts. A preferred alkaline material for use in elevating the pH of the aqueous solution in the present invention is Cement Kiln Dust (CKD), and a preferred source of aqueous magnesium ions is reject water from a desalination plant.
Bibliography:Application Number: CN2014832136