Physical concentration and phosphorus reduction method for skarn-type high-phosphorus molybdenum ore

The invention discloses a physical concentration and phosphorus reduction method for a skarn-type high-phosphorus molybdenum ore. The physical concentration and phosphorus reduction method comprises the following steps of (1) crushing, namely crushing raw ores by using a crusher, sieving, and return...

Full description

Saved in:
Bibliographic Details
Main Authors YAN WEIPING, WANG XIUFEN, MAO YILIN, YANG JINZHONG, CHEN XIAOQING, LIU NENGYUN
Format Patent
LanguageChinese
English
Published 09.03.2016
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a physical concentration and phosphorus reduction method for a skarn-type high-phosphorus molybdenum ore. The physical concentration and phosphorus reduction method comprises the following steps of (1) crushing, namely crushing raw ores by using a crusher, sieving, and returning a +3mm-grade raw ore to crush until the particle size of the raw ore is up to the -3mm grade; (2) grinding the ores, namely adding the crushed -3mm-grade raw ore into raw ore grinding equipment to carry out closed-circuit ore grinding operation, meanwhile, adding 500-1000g/t of water glass and 250-800g/t of a phosphate mineral inhibitor into a grinding machine, and grinding the raw ore until the particle size is up to the -0.075mm grade and the phosphorus content is up to 55-75%; (3) carrying out roughing operation; (4) carrying out scavenging operation; (5) regrinding a roughed molybdenum concentrate, namely adding 100-280g/t of a sulfur inhibitor and 150-300g/t of a phosphate mineral inhibitor to regrind the