Flake Graphite Iron And Methods Of Preparing Flake Graphite Iron

The present invention provides a flake graphite iron and a method of preparing the flake graphite iron. The flake graphite iron comprises, relative to the total weight, and by weight, 2.6% to 3.2% of carbon C, 1.6% to 2.0% of silicon Si, 0.6% to 0.8% of manganese Mn, 0.1% to 0.15% of sulfur, at leas...

Full description

Saved in:
Bibliographic Details
Main Authors DONG SEOB SHIM, SIK YANG, JONG KWON CHUNG, KI HWAN JUNG, YOUNG KYU JU, YE NI SEUL LEE, JAE HYOUNG HWANG
Format Patent
LanguageEnglish
Published 26.08.2015
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The present invention provides a flake graphite iron and a method of preparing the flake graphite iron. The flake graphite iron comprises, relative to the total weight, and by weight, 2.6% to 3.2% of carbon C, 1.6% to 2.0% of silicon Si, 0.6% to 0.8% of manganese Mn, 0.1% to 0.15% of sulfur, at least 0 to 0.05% of phosphorus and the residual iron Fe. The weight ratio of the carbon and sulfur(C/S) is 18 to 27, and the weight ratio of the manganese and sulfur (Mn/S) is 4 to 8. By adjusting the weight ratio of the carbon and sulfur and the weight ratio of the manganese and sulfur, the high intensity of flake graphite iron can be obtained.
Bibliography:Application Number: CN201510083860