Preparation method of colored superhydrophobic coating with outstanding corrosion resistance
The invention provides a preparation method of a colored superhydrophobic coating with outstanding corrosion resistance. In the method, colored stearate hydrophobic powder is prepared by the chemical precipitation method by using sodium stearate as a precursor, inorganic salt as a reaction substrate...
Saved in:
Main Authors | , , , , |
---|---|
Format | Patent |
Language | English |
Published |
03.06.2015
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention provides a preparation method of a colored superhydrophobic coating with outstanding corrosion resistance. In the method, colored stearate hydrophobic powder is prepared by the chemical precipitation method by using sodium stearate as a precursor, inorganic salt as a reaction substrate, and water as a reaction solvent; stearate hydrophobic powder is dispersed into absolute ethyl alcohol to form suspension; a colored super-hydrophobic coating is prepared by the coating method by using nitrogen as carrier gas and a stainless steel block as a substrate. The contact angle test shows that the contact angle of the colored stearate coating to deionized water and acidic and alkaline water drop is more than 150 degrees; after the coating is soaked for 30 days through 3.5wt% of a NaCl water solution, the contact angle is still more than 150 degrees, so that high super-hydrophobic performance is maintained; the coating used as a super-hydrophobic material is high in corrosion resistance and has a good commerce prospect in the technical field of a special soakage interface. |
---|---|
Bibliography: | Application Number: CN2015143283 |