Flux-cored wire for gas-shielded arc welding, method for welding steel for very low temperature use, and method for manufacturing weld joint
There is provided a flux-cored wire capable of obtaining a weld metal having excellent low temperature toughness and improving welding efficiency, in which preheating performed for preventing cold cracking can be omitted or simplified. The flux-cored wire includes one or more of CaF2 , BaF2 , SrF2 ,...
Saved in:
Main Authors | , , , |
---|---|
Format | Patent |
Language | English |
Published |
20.05.2015
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | There is provided a flux-cored wire capable of obtaining a weld metal having excellent low temperature toughness and improving welding efficiency, in which preheating performed for preventing cold cracking can be omitted or simplified. The flux-cored wire includes one or more of CaF2 , BaF2 , SrF2 , MgF2 , and LiF and, when a total amount thereof is defined as alpha, the alpha is 2.0% to 7.0%, by mass%, with respect to a total mass of the flux-cored wire, one or more of a Ti oxide, a Si oxide, a Mg oxide, an A1 oxide, a Zr oxide, and a Ca oxide are included in the flux-cored wire, and when a total amount thereof is defined as beta, the beta is 0.2% to 0.9%, by mass%, with respect to the total mass of the flux-cored wire, a ratio of an amount of the CaF2 with respect to the alpha is 0.90 or more, and a ratio of the beta with respect to the is 3.0 or more and 15.0 or less. |
---|---|
Bibliography: | Application Number: CN20141643455 |