Method for improving grain size of TP347HFG wrought pipe billet
The invention relates to a method for improving grain size of a TP347HFG wrought pipe billet, belonging to the field of forging. The method is characterized by comprising the following steps: heating a forging material to 1100 DEG C above, keeping the temperature for 3-3.5 hours until the internal a...