Preparation method of catalyst for improving yield of diesel oil produced by catalytic cracking
The invention discloses a preparation method of a catalyst for improving the yield of diesel oil produced by catalytic cracking. The preparation method comprises the following steps: with a mixture of kaolin and diatomite subjected to acid treatment as a raw material, adding chemical water, structur...
Saved in:
Main Authors | , , , , , , , , , |
---|---|
Format | Patent |
Language | English |
Published |
14.01.2015
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention discloses a preparation method of a catalyst for improving the yield of diesel oil produced by catalytic cracking. The preparation method comprises the following steps: with a mixture of kaolin and diatomite subjected to acid treatment as a raw material, adding chemical water, structural auxiliaries, a dispersing agent and/or a reinforcing agent into the mixture, and performing mixed pulping and spraying to obtain microspheres; roasting the sprayed microspheres, mixing the roasted microspheres with a guiding agent, sodium silicate and sodium hydroxide in a certain ratio, and performing a crystallization reaction under hydrothermal conditions, thereby obtaining a crystallization product with a pore structure and excellent abrasion resistance and with a 20%-30% NaY molecular sieve, wherein the crystallization product, namely the in-situ crystallized microspheres, can be taken as a precursor for preparing the catalytic cracking catalyst; and exchanging the in-situ crystallized microspheres with ammonium salt and rare earth to obtain the catalytic cracking catalyst for improving the yield of diesel oil. |
---|---|
Bibliography: | Application Number: CN20131292121 |