Anisotropic electromagnetic steel sheet and method for producing same

Provided is an anisotropic electromagnetic steel sheet comprising, by mass%, 0.005% or less of C, 0.1% to 2.0% of Si, 0.05 to 0.6% of Mn, 0.100% or less of P, and 0.5% or less of Al, wherein the content of nonmagnetic precipitate AlN having an average diameter of 10 to 200 nm is, by number density,1...

Full description

Saved in:
Bibliographic Details
Main Authors FUJIKURA MASAHIRO, ATAKE MAKOTO, USHIGAMI YOSHIYUKI, KANAO SHINICHI, HORI KOJIRO, ICHIE TAKERU, MURAKAWA TESSHU
Format Patent
LanguageChinese
English
Published 16.07.2014
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Provided is an anisotropic electromagnetic steel sheet comprising, by mass%, 0.005% or less of C, 0.1% to 2.0% of Si, 0.05 to 0.6% of Mn, 0.100% or less of P, and 0.5% or less of Al, wherein the content of nonmagnetic precipitate AlN having an average diameter of 10 to 200 nm is, by number density,10 precipitates/[mu]m or less, and the average flux density in the rolling direction and the direction perpendicular to rolling is 1.75 T or greater. This anisotropic electromagnetic steel sheet can be produced by two methods, the method of hot rolling and annealing at a temperature between 750 DEG C and the Ac1 transformation temperature and the method of self-annealing at a coil take-up temperature of 780 DEG C or greater.
Bibliography:Application Number: CN201280055225