Preparation method for titanium dioxide pigment
The invention provides a preparation method for a titanium dioxide pigment. The method comprises the following steps: a titanium dioxide powder material is subjected to pulping and dispersion processing, a titanium dioxide pulp material is obtained, the pH value of the pulp material is adjusted to 9...
Saved in:
Main Authors | , , , , , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
09.04.2014
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention provides a preparation method for a titanium dioxide pigment. The method comprises the following steps: a titanium dioxide powder material is subjected to pulping and dispersion processing, a titanium dioxide pulp material is obtained, the pH value of the pulp material is adjusted to 9.0-11.0, the pulp material is heated to 80-100 DEG C, a sodium silicate solution is added with an addition amount of being 1.0-5.0% of TiO2 mass in the pulp material in terms of SiO2, the temperature of the system is kept unchangeable, the pH value of the pulp material is adjusted to 3.0-5.0, slaking is carried out, the pH value of the pulp material is adjusted to 6.0-9.0, a solution containing phosphate radical compounds with an addition amount of being 1.0-4.0% of TiO2 mass in the pulp material in terms of P2O5 is added, at the same time, a solution containing aluminum compounds is added to keep the pH value of the pulp material being 5.0-9.0, the addition amount of the added solution containing aluminum compound |
---|---|
Bibliography: | Application Number: CN20131653529 |