Method for heat application of low-alkalinity casting residue in steel-making

The invention provides a method for heat application of low-alkalinity casting residue in steel-making. The method comprises the following steps that: 5 to 7kg/t of low-alkalinity casting reside of steel slag is added to a converter along with semi-steel under a hot steel state in order to fully uti...

Full description

Saved in:
Bibliographic Details
Main Authors MA YANLONG, YANG CHUNLEI, CAO ZHONG, ZHAO WEIDONG, ZHANG ZHUXIONG, WANG DINGSHU, SU MEIPING, JI HONGGANG
Format Patent
LanguageChinese
English
Published 27.03.2013
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention provides a method for heat application of low-alkalinity casting residue in steel-making. The method comprises the following steps that: 5 to 7kg/t of low-alkalinity casting reside of steel slag is added to a converter along with semi-steel under a hot steel state in order to fully utilize the heat of the molten casting residue, and the slag can be quickly generated by blowing for 2 minutes. By adopting the method, the complex slag forming constituent and heating agent requested in a conventional semi-steel smelting process are saved, and the production cost is reduced; the high-alkalinity slag can be quickly formed at low temperature in accordance with the slag formation system; the content of phosphorus of 0.35 to 0.80% in the molten ion can be quickly removed within the normal smelting period, and the final requirement of steel grade can be met; all casting residues in steel making are basically recycled, so that the pressure of residue discharge to the environment and the handling cost can b
Bibliography:Application Number: CN20121500164