Method for preparing copper sulphide nanosheet
The invention discloses a method for preparing a copper sulphide nanosheet, comprising the following steps of: dissolving copper chloride and surfactant in deionized water to prepare a solution A; and dissolving thioacetamide in the deionized water to prepare a solution B; 2) mixing two solutions, i...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
26.09.2012
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention discloses a method for preparing a copper sulphide nanosheet, comprising the following steps of: dissolving copper chloride and surfactant in deionized water to prepare a solution A; and dissolving thioacetamide in the deionized water to prepare a solution B; 2) mixing two solutions, i..e. the solution A and the solution B serving as a reaction solution to carry out water bath reaction to prepare a hexagon copper sulphide nanosheet; and controlling the side length of the copper sulphide nanosheet to be between 55 and 140nm and the thickness to be between 8 and 20nm through controlling a reaction condition. The method has the characteristics of easiness in acquisition of raw materials, simple equipment, low cost, simplicity in operation, effectiveness, quickness and the like; and the prepared copper sulphide nanosheet is ordered in appearance, high in dispersibility, yield rate and stability, controllable in sizes and suitable for large-scale industrial production. The prepared copper sulphide na |
---|---|
Bibliography: | Application Number: CN2012160199 |