Method for improving thickness of decarburized layer of small square billet of tire cord steel

The invention belongs to the technical field of the metallurgy and processing of iron and steel and provides a method for improving the thickness of a decarburized layer of a small square billet of tire cord steel. The tire cord steel is produced by adopting the technological processes of heating, r...

Full description

Saved in:
Bibliographic Details
Main Authors WU NIANCHUN, LIU CHAOXIA, WEI ZHIWEN, FENG GONGXIONG, ZHENG JIANQIANG, LI YUHUA, YIN YUQUN
Format Patent
LanguageChinese
English
Published 04.07.2012
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention belongs to the technical field of the metallurgy and processing of iron and steel and provides a method for improving the thickness of a decarburized layer of a small square billet of tire cord steel. The tire cord steel is produced by adopting the technological processes of heating, rough rolling, intermediate rolling, pre-finishing, finishing and air cooling. The method for improving the thickness of the decarburized layer of the small square billet of the tire cord steel comprises the following steps that: prior to the technological process of heating, corner grinding or whole-stripping treatment is carried out on the square billet; the total detention time for the square billet in a heating furnace is less than 150 min, and the detention time in a soaking section is lessthan 45 min; fuel gas is fully combusted in the soaking section, wherein the air-fuel ratio in a heating I section is set to be 1.1, the air-fuel ratio in a heating II section is set to be 0.9, and the air-fuel ratio in the s