Blank for high-whiteness vitrified tiles

The invention discloses a blank for high-whiteness vitrified tiles, which is prepared by the following components by weight parts: 20-35 parts of albite, 1-3 parts of feldspar, 1-3 parts of calcite, 6-12 parts of talc, 1-3 parts of potassium nitrate, 25-40 parts of kaolin, 30-45 parts of quartz, 10-...

Full description

Saved in:
Bibliographic Details
Main Author CHEN XINJI
Format Patent
LanguageChinese
English
Published 04.07.2012
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a blank for high-whiteness vitrified tiles, which is prepared by the following components by weight parts: 20-35 parts of albite, 1-3 parts of feldspar, 1-3 parts of calcite, 6-12 parts of talc, 1-3 parts of potassium nitrate, 25-40 parts of kaolin, 30-45 parts of quartz, 10-25 parts of boric acid, 8-15 parts of iron sesquioxide, 2-5 parts of cobalt oxide, 3-6 parts of manganese oxide and 3-8 parts of zirconium silicate; the formula of the invention is obtained by improvement on the basis of the traditional formula, and the vitrified tiles produced by taking the blank of the invention as the raw materials have few micropores and have the characteristics of high whiteness, high hardness and high wear resistance.
Bibliography:Application Number: CN20111417824