Process for producing mass colouration float glass by furnace slag powder

The invention provides a process for producing mass colouration float glass by furnace slag powder, which comprises the following steps of: A, weighing the following raw materials in percentage by weight: 3 to 6 percent of furnace slag powder, 50 to 60 percent of silica sand, 16 to 20 percent of sod...

Full description

Saved in:
Bibliographic Details
Main Authors ZHANG QI, ZHOU HE, DONG QINGSHI, LIU LIFEI, XIAO LEI, YANG JIANJUN, WAN JUNPENG
Format Patent
LanguageChinese
English
Published 23.05.2012
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention provides a process for producing mass colouration float glass by furnace slag powder, which comprises the following steps of: A, weighing the following raw materials in percentage by weight: 3 to 6 percent of furnace slag powder, 50 to 60 percent of silica sand, 16 to 20 percent of soda, 9 to 13 percent of dolomite, 3 to 6 percent of limestone, 3 to 6 percent of feldspar, 0.3 to 0.8 percent of mirabilite and 0.01 to 0.05 percent of carbon powder; B, sequentially adding the raw materials into a mixer according to the sequence and uniformly mixing the raw materials to obtain a mixture; and C, melting, forming and annealing the mixture at a high temperature of 1,600 DEG C by a melting furnace to obtain the mass colouration float glass. In the process provided by the invention, furnace slags discharged as the waste in the metallurgical industry are utilized; after being processed, the furnace slags are applied to a production line of the mass colouration float glass as a colouring additive; and othe
Bibliography:Application Number: CN20101546521