Preparation method of zinc-aluminium seamless flux-cored wire
The invention provides a preparation method of a zinc-aluminium seamless flux-cored wire. The method provided by the invention is characterized by comprising the following steps: smelting raw materials such as zinc, aluminium and the like, and casting the melt into an ingot; after riser removal and...
Saved in:
Main Authors | , , , , , , , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
26.10.2011
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention provides a preparation method of a zinc-aluminium seamless flux-cored wire. The method provided by the invention is characterized by comprising the following steps: smelting raw materials such as zinc, aluminium and the like, and casting the melt into an ingot; after riser removal and scalping, putting the ingot into a nitrogen protection furnace and carrying out shpheroidizing annealing in the nitrogen protection furnace at 180-230 DEG C for 1-2 hours; blending a core flux into paste by virtue of an organic solvent and filling the paste in a pressure injector; then putting the zinc-aluminium alloy ingot into a dedicated extrusion die, connecting the die to the pressure injector, and starting the extrusion die to directly extrude welding wire which has the diameter phi of 5.0-12.0mm and has a core of the flux and a sheath of the zinc-aluminium alloy; and then performing drawings many times to obtain the finished product. The flux-cored wire manufactured by the method is characterized in that the |
---|---|
Bibliography: | Application Number: CN20111166271 |