Summary:The present invention provides a process for production of an aluminum wheel, which makes it possible, even when non-chromate surface treatment is conducted after casting, to attain sufficient tight adhesion between an aluminum wheel and a non-chromate coating and sufficient corrosion resistance. A process for production of an aluminum wheel, is characterized by comprising the cleaning step of etching the surface of an aluminum wheel chemically with an alkaline cleaning fluid containing an alkaline builder, an organic builder and a chelating agent until the atomic ratio of metallic Si to oxide Si on the surface of the aluminum wheel becomes 0.01 to 9. In cleaning the surface of an aluminum wheel, the process can dispense with shot blasting.