Low-alloy abrasion-resistant steel and manufacturing method thereof
The invention relates to low-alloy abrasion-resistant steel and a manufacturing method thereof. The low-alloy abrasion-resistant steel comprises the following compositions in percentage by weight: C: 0.12-0.24, Si: 0.20-0.70, Mn: 1.00-1.80, P: not more than 0.010, S: not more than 0.005, Cr: 0.30-1....
Saved in:
Main Authors | , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
04.05.2011
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention relates to low-alloy abrasion-resistant steel and a manufacturing method thereof. The low-alloy abrasion-resistant steel comprises the following compositions in percentage by weight: C: 0.12-0.24, Si: 0.20-0.70, Mn: 1.00-1.80, P: not more than 0.010, S: not more than 0.005, Cr: 0.30-1.40, Mo: 0.10-0.50, Ni: 0-0.80, Cu: 0-0.50, Al: 0.02-0.06, Ti: 0.005-0.02, and the balance of Fe and inevitable impurities. Due to reasonable design of element varieties and content and addition of a proper amount of alloy elements, the abrasion-resistant steel achieves the advantages of high yield strength, high hardness, better toughness, and favorable abrasion resistance. |
---|---|
Bibliography: | Application Number: CN20091197635 |