High temperature oxidation resistant grid section and preparation method thereof
The invention provides a high temperature oxidation resistant grid section, comprising the following components by weight percent: 0.3-0.6% of C, 0.2-0.4% of N, 22-25% of Cr, 0.3-0.5% of Si, 3-4% of Mn, 6-8% of Ni, 0.001-0.002% of B, less than 0.01% of Zr, the balance Fe. The grid section of the inv...
Saved in:
Main Authors | , , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
15.02.2012
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention provides a high temperature oxidation resistant grid section, comprising the following components by weight percent: 0.3-0.6% of C, 0.2-0.4% of N, 22-25% of Cr, 0.3-0.5% of Si, 3-4% of Mn, 6-8% of Ni, 0.001-0.002% of B, less than 0.01% of Zr, the balance Fe. The grid section of the invention is prepared by adopting melting, refining, alloying and casting stages. The grid section of the invention has high rigidity and better impact property, distortion resistance capacity at high temperature is improved, and meanwhile corrosion resistance is also improved, and the oxidation film of the grid section of the invention contains no Mn3O4, so that the oxidation film thereof is stable at high temperature and has better compactness and continuity, bonding degree with base material is higher, and the grid section has excellent oxidation resistance and is superior to the existing grid section. |
---|---|
Bibliography: | Application Number: CN20101161371 |