The invention relates to a method for preparing AZ91D magnesium alloy semi-solid sizing agent by rotating pouring, which is characterized in that AZ91D magnesium alloy is melted and refined in a smelting maintaining furnace, then cooled to 630-650 DEG C, and insulated for 10-30 minutes; a stainless...

Full description

Saved in:
Bibliographic Details
Main Authors YANG XIANGJIE, WANG XIAOKANG, CHENG SHANGXU, YE HAN, WAN ZHENGDONG, GUO HONGMIN, WANG MING
Format Patent
LanguageChinese
English
Published 11.02.2009
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention relates to a method for preparing AZ91D magnesium alloy semi-solid sizing agent by rotating pouring, which is characterized in that AZ91D magnesium alloy is melted and refined in a smelting maintaining furnace, then cooled to 630-650 DEG C, and insulated for 10-30 minutes; a stainless steel rotating pouring tube is preheated to 60-80 DEG C, with the rotating speed of the pouring tube controlled at 0-105r/min, and the inclination of the rotating pouring tube being 20-30 degrees; then the AZ91D magnesium alloy melt is poured into the rotating tube through a deflection tube; a crystallizer is preheated to 470-500 DEG C; the AZ91D magnesium alloy melt enters the crystallizer through the rotating pouring tube, and insulated for 5-15 minutes. The method for preparing the AZ91D magnesium alloy semi-solid sizing agent by rotating pouring has a simple device, low cost, convenient operation, high practicality; the prepared AZ91D magnesium alloy semi-solid sizing agent has fine grain organization and even
Bibliography:Application Number: CN20081107093