Low temperature-resistant dry-resistant antistatic mixed solution preparation method

The invention relates to a method for preparing mixing solution, which is characterized in that it comprises following steps: putting nanohyperconductive CaCL2 crystal 2-5%, alaum crystal 1-2%, conductive MgCl2 crystal 0.2- 1% into mixing container and cold mixing for 5- 10 minutes to form homogenou...

Full description

Saved in:
Bibliographic Details
Main Author DECHENG XU
Format Patent
LanguageEnglish
Published 01.08.2007
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention relates to a method for preparing mixing solution, which is characterized in that it comprises following steps: putting nanohyperconductive CaCL2 crystal 2-5%, alaum crystal 1-2%, conductive MgCl2 crystal 0.2- 1% into mixing container and cold mixing for 5- 10 minutes to form homogenous powder, adding AT antistatic agent 0.2- 1% and clean water 90-95% into container, heating to 40- 50 Deg. C; putting prepared powder into this solution, stirring throughly for 5- 10 minutes. The mixing solution possesses excellent effect of low- temperature resistance and dry resistance.
Bibliography:Application Number: CN2006138125