NEW AND NOVEL ENGINEERING RESIN THERMOPLASTIC SILICONE VULCANIZATES

A method for preparing a modified thermoplastic resin by mixing a thermoplastic resin having a t g of 95°C or greater and having a melt processing temperature of 250°C or greater with a silicone base comprised of 100 parts by weight of a diorganopolysiloxane gum and having an average of at least 2 a...

Full description

Saved in:
Bibliographic Details
Main Authors ROMENESKO, DAVID, MEHTA, VEERAG YAGNIK
Format Patent
LanguageEnglish
French
Published 29.04.2012
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A method for preparing a modified thermoplastic resin by mixing a thermoplastic resin having a t g of 95°C or greater and having a melt processing temperature of 250°C or greater with a silicone base comprised of 100 parts by weight of a diorganopolysiloxane gum and having an average of at least 2 alkenyl groups per molecule in conjunction with 0 to 50 parts by weight of a reinforcing filler along with a radical initiator. The silicone base and this combination are dynamically vulcanized to cure the silicone base at an elevated temperature.
Bibliography:Application Number: CA20112751862