METHOD FOR PRODUCING A MAGNESIUM HOT STRIP

The invention relates to a method for producing a magnesium hot strip, in which a melt from a magnesium alloy is continuously cast to form a roughed strip with a thickness of maximum 50 mm, and in which the cast roughed strip is hot-rolled directly from the cast heat at a hot-rolling initial tempera...

Full description

Saved in:
Bibliographic Details
Main Authors KAWALLA, RUDOLF, PIRCHER, HANS
Format Patent
LanguageEnglish
French
Published 01.12.2009
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention relates to a method for producing a magnesium hot strip, in which a melt from a magnesium alloy is continuously cast to form a roughed strip with a thickness of maximum 50 mm, and in which the cast roughed strip is hot-rolled directly from the cast heat at a hot-rolling initial temperature of at least 250 .degree.C and maximum 500 .degree.C to form a hot strip with a final thickness of maximum 4 mm, whereby in the first hot-rolling pass a reduction in the thickness of at least 15 % is achieved. With the method according to the invention, magnesium sheets with improved deformability can be produced with reduced manufacturing effort and expenditure.
Bibliography:Application Number: CA20012425580