METHOD OF MAKING A MOLDED PLASTIC CONTAINER

A polyethylene terephthalate (PET) preform (11) having a capped cylindrical body (13), a threaded top and collared neck (19) is preheated to soften the PET.The preform (11) is placed in a split mold (26) whose walls are heated to a temperature between 150.degree.C and 177.degree.C. A stretch rod (35...

Full description

Saved in:
Bibliographic Details
Main Author RUPPMAN, KURT H., SR
Format Patent
LanguageEnglish
French
Published 22.08.2000
Edition6
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A polyethylene terephthalate (PET) preform (11) having a capped cylindrical body (13), a threaded top and collared neck (19) is preheated to soften the PET.The preform (11) is placed in a split mold (26) whose walls are heated to a temperature between 150.degree.C and 177.degree.C. A stretch rod (35), inserted through the top of the preform (11), stretches the preform (11) axially until the preform is the length of the final product (49). The preform (11) is expanded using compressed ambient air, and is molded against the walls (27, 29) of the mold (26). The air is vented, and dry nitrogen at a temperature below -50.degree.C is injected into the molded preform (47) to purge and cool the molded preform (47) while maintaining pressure of at least 520 kPag. The molded preform (47) is held against the mold (36) to anneal the inner and outer surfaces of the molded preform (47). The nitrogen supply is shut off and the final product (49) is released from the mold (26).
Bibliography:Application Number: CA19962191093