ALUMINUM NITRIDE SINTERED BODY WITH HIGH THERMAL CONDUCTIVITY AND ITS PREPARATION

An aluminum nitride sintered product with a high thermal conductivity (at least 100 W/m.K) can be prepared at a sintering temperature of less than 1850 .degree.C (often less than 1650 .degree.C) using a sinterable combination of aluminum nitride powder with at least three sintering aids. The sinteri...

Full description

Saved in:
Bibliographic Details
Main Authors HASHIMOTO, NOBORU, ZHAO, JUNHONG, GUITON, THERESA A, RAFANIELLO, WILLIAM, CHIAO, YI-HUNG
Format Patent
LanguageEnglish
French
Published 26.01.1995
Edition6
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:An aluminum nitride sintered product with a high thermal conductivity (at least 100 W/m.K) can be prepared at a sintering temperature of less than 1850 .degree.C (often less than 1650 .degree.C) using a sinterable combination of aluminum nitride powder with at least three sintering aids. The sintering aids include a source of a rare earth metal oxide, a source of an alkaline earth metal oxide, a boron source and, optionally, a source of aluminum oxide. The sinterable combinations may also be used to prepare cofired, multilayer substrates.
Bibliography:Application Number: CA19942171548