GREEN STRENGTH OF ELASTOMER BLENDS
The green strength of elastomer blends of natural or synthetic cis-1,4-polyisoprene and synthetic elastomers is improved by including an ionogenic group having the formula Where X1 and X2 are selected from the group consisting of hydrogen, methyl, carboxyl, fluorine, chlorine, bromine, and iodine, R...
Saved in:
Main Authors | , |
---|---|
Format | Patent |
Language | English French |
Published |
29.09.1981
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The green strength of elastomer blends of natural or synthetic cis-1,4-polyisoprene and synthetic elastomers is improved by including an ionogenic group having the formula Where X1 and X2 are selected from the group consisting of hydrogen, methyl, carboxyl, fluorine, chlorine, bromine, and iodine, R, is H, C, through C 10, - (CH2)? COOH, n - 0 to 4, or a halogen, m is 0 to 11, and A is OH, OM or NH2 where M is a metal selected from groups 1A, 2A, 3A or 2B of the Periodic Table. The said ionogenic group can be incorporated into the chain of the synthetic elastomer a? through any conventional polymerization of the monomers forming the synthetic elastomer. Generally, the blends have greatly improved green strength as compared to rubber blends known to the art. The blends of the present invention are of particular use in tires and tire components, as well as in conveyor belts, hoses, and the like. |
---|---|
Bibliography: | Application Number: CA19770279820 |